Characteristics of
2011 Aluminum round bar rod
2011 is a typical hard aluminium alloy in the aluminium-copper-magnesium system. It is a cold-drawn or refined aluminium product. Because of the addition of lead and bismuth, it is the most free-cutting alloy product with excellent machinability.
The available states are: T3, T4, T8, etc.
Applications of
2011 Aluminum round bar rod
Aluminum alloy 2011 is widely used in automotive oil system accessories, clock parts, gears, machine parts, pipes, cable TV adapters, camera parts, instrument shafts, national defense products, industrial connectors,etc.
Chemical composition of
2011 Aluminum round bar rod
|
Si |
Fe |
Cu |
Mg |
Pb |
Bi |
Zn |
Ti |
single |
Total |
|
0.4 |
0.7 |
5.0-6.0 |
- |
0.20-0.6 |
0.20-0.6 |
0.3 |
- |
0.05 |
0.15 |
Physical Properties of
2011 Aluminum round bar rod
Density
kg•m-3 |
Coefficient of thermal expansion
µm•(m•K)-1 |
Elastic modulus
E/Pa |
Conductivity
(20℃/IACS) |
Thermal Conductivity
20℃/W•(m•K)-1 |
Resistivity
20℃/nΩ•m |
|
2.82 |
23.1 |
70 |
45 |
173 |
38 |
Standard for Heat Treatment of
2011 Aluminum round bar rod
|
Annealing specification |
Solid solution temperature |
Prescription Specification |
|
413℃ |
524℃ |
160℃*14h |